General Information

The PrimeWeld TIG225X is an AC/DC TIG welder with pulse, located in the Metal Shop. It also does DC stick welding. Use AC for aluminum and DC for steel and stainless steel.

Report equipment issues on Slack in #general or #shop-metal.

PrimeWeld TIG225X in the Metal Shop.

Specifications

Specification Details
Input 120V or 240V, single-phase
TIG output 10–225A on 240V; 10–140A on 120V
Stick output DC stick (MMA)
Duty cycle (TIG) 40% at maximum output; 100% at 155A on 240V or 108A on 120V
Arc start High-frequency (no-touch) start
Amperage control Front panel or foot pedal
Shielding gas Pure argon

Duty cycle is how much of a 10-minute period the machine can weld at that current. At maximum output, weld for 4 minutes and let it cool for 6. If the machine overheats, its thermal protection stops output until it cools.

Orientation and Access

Training is required to use the TIG welder. Complete the general space orientation first. See Welding Equipment for welding orientation, and check the event calendar for upcoming training.

Safety

Follow the Metal Shop safety requirements for helmets, gloves, jackets, ventilation, and flammable materials.

  • The TIG arc gives off strong ultraviolet light. Cover all exposed skin, and close the weld curtain.
  • The tungsten, torch cup, and workpiece stay hot after you stop welding.
  • Clean metal before welding. Do not weld galvanized, plated, or painted metal without removing the coating first.
  • If the tungsten touches the weld pool or filler rod, stop and regrind or replace it. A contaminated tungsten gives an unstable arc.

Controls

Selector Switches

Switch Function
TIG / MMA TIG welding or DC stick welding.
AC / DC In TIG mode: AC for aluminum and magnesium, DC for steel, stainless steel, and most other metals.
2T / 4T 2T: press and hold the torch switch to weld, release to stop. 4T: press to start, release to weld, press again to start the down slope, release to stop. Use 4T for long welds without a foot pedal.
Pulse (Off / Low / High) Off: standard TIG. Low and High set the pulse frequency range.

Control Dials

Dial Function
Welding Current Main amperage. With the foot pedal connected, this sets the maximum the pedal can reach.
Pre-Flow Gas flow before the arc starts.
Start Current Current when the arc strikes. Lower it for thin sheet metal.
Up Slope Time to rise from start current to welding current.
Base Current In pulse mode, the low current level, as a percentage of welding current.
Pulse Frequency In pulse mode, how many times per second the current switches between peak and base.
Pulse Duty In pulse mode, how much of each pulse is at peak current. Higher gives more heat and penetration; lower is safer for thin material.
Down Slope Time to drop from welding current to end current.
End Current Current at the end of the weld, to fill the crater.
Post Flow Gas flow after the arc stops. Protects the hot tungsten and weld while they cool.
AC Frequency In AC mode, a higher frequency gives a narrower, more focused arc.
AC Balance In AC mode, the balance between cleaning action, which removes oxide from aluminum, and penetration.

Setup

  1. Make sure the machine is off.
  2. Set TIG / MMA to TIG. Set AC / DC for your metal.
  3. Fit the tungsten. Use a collet and collet body that match the tungsten diameter, and a cup sized for the job. The kit includes 1/16" and 3/32" collets and #5, #6, and #7 cups.
  4. Clamp the ground to clean, bare metal close to the joint.
  5. Open the argon cylinder valve and set the flow on the regulator.
  6. Plug in the foot pedal, or set 2T / 4T to use the torch switch.
  7. Turn the machine on and set the welding current and post flow.


Shutting Down

  1. Let the post flow finish before you lift the torch away.
  2. Turn off the machine.
  3. Close the argon cylinder valve.
  4. Hang the torch and coil the leads. Let the torch cool before storing it.