TIG Welder: Difference between revisions
Describe our 2022-2023 unit on 240V, add starting settings for steel and aluminum |
Match control dials to our panel, add ranges and overheat light |
||
| Line 1: | Line 1: | ||
<!-- TODO: | <!-- TODO: add where tungsten and filler rod are kept. Control Dials table confirmed against a photo of our panel (model label TIG225ACDCP), November 2026. --> | ||
== General Information == | == General Information == | ||
| Line 81: | Line 81: | ||
=== Control Dials === | === Control Dials === | ||
These are the dials on our machine's panel, in panel order. The line drawn across the panel between the two rows shows where each setting acts during a weld. | |||
{| class="wikitable" | {| class="wikitable" | ||
|- | |- | ||
! Dial | ! Dial | ||
! Range | |||
! Function | ! Function | ||
|- | |- | ||
| '''Start Current''' | | '''Start Current''' | ||
| 10–225A | |||
| Current when the arc strikes. Lower it for thin sheet metal. | | Current when the arc strikes. Lower it for thin sheet metal. | ||
|- | |- | ||
| '''Up Slope''' | | '''Up Slope''' | ||
| Up to 10 s | |||
| Time to rise from start current to welding current. | | Time to rise from start current to welding current. | ||
|- | |- | ||
| ''' | | '''Welding Current''' | ||
| | | 10–225A | ||
| Main amperage, shown on the AMP display. With the foot pedal connected, this sets the maximum the pedal can reach. | |||
| | |||
|- | |- | ||
| '''Down Slope''' | | '''Down Slope''' | ||
| 0–25 s | |||
| Time to drop from welding current to end current. | | Time to drop from welding current to end current. | ||
|- | |- | ||
| '''End Current''' | | '''End Current''' | ||
| 10–225A | |||
| Current at the end of the weld, to fill the crater. | | Current at the end of the weld, to fill the crater. | ||
|- | |- | ||
| '''AC Frequency''' | | '''AC Frequency''' | ||
| 40–200 Hz | |||
| In AC mode, a higher frequency gives a narrower, more focused arc. | | In AC mode, a higher frequency gives a narrower, more focused arc. | ||
|- | |- | ||
| '''AC Balance''' | | '''AC Balance''' | ||
| 10–90% | |||
| In AC mode, the balance between cleaning action, which removes oxide from aluminum, and penetration. | | In AC mode, the balance between cleaning action, which removes oxide from aluminum, and penetration. | ||
|- | |||
| '''Pre-Flow''' | |||
| Up to 3 s | |||
| Gas flow before the arc starts. | |||
|- | |||
| '''Base Current''' | |||
| Up to 95% | |||
| In pulse mode, the low current level, as a percentage of welding current. | |||
|- | |||
| '''Pulses Per Second''' | |||
| Up to 200 Hz | |||
| In pulse mode, how many times per second the current switches between peak and base. | |||
|- | |||
| '''Pulse Duty''' | |||
| From 10% | |||
| In pulse mode, how much of each pulse is at peak current. Higher gives more heat and penetration; lower is safer for thin material. | |||
|- | |||
| '''Post Flow''' | |||
| From 0 s | |||
| Gas flow after the arc stops. Protects the hot tungsten and weld while they cool. | |||
|} | |} | ||
The '''O.C''' light next to the display comes on when the machine overheats or is overloaded. Stop and let it cool before welding again. | |||
== Setup == | == Setup == | ||
Latest revision as of 15:36, 22 November 2026
General Information
The PrimeWeld TIG225X is an AC/DC TIG welder with pulse, located in the Metal Shop. It also does DC stick welding. Use AC for aluminum and DC for steel and stainless steel.
Our machine is the 2022–2023 version. It runs on 240V and uses the CK Worldwide 17-series air-cooled torch with Superflex hose that came with it. PrimeWeld's current model adds AC waveform selection and a spot-weld mode; ours does not have them.
Report equipment issues on Slack in #general or #shop-metal.

Specifications
| Specification | Details |
|---|---|
| Input | 240V, single-phase (the machine also accepts 120V, but we run it on 240V) |
| TIG output | 10–225A |
| Stick output | DC stick (MMA) |
| Duty cycle (TIG) | 40% at 225A |
| Torch | CK Worldwide 17-series, air-cooled, Superflex hose |
| Arc start | High-frequency (no-touch) start |
| Amperage control | Front panel or foot pedal |
| Shielding gas | Pure argon |
Duty cycle is how much of a 10-minute period the machine can weld at that current. At 225A, weld for 4 minutes and let it cool for 6. At lower currents you can weld longer. If the machine overheats, its thermal protection stops output until it cools.
Orientation and Access
Training is required to use the TIG welder. Complete the general space orientation first. See Welding Equipment for welding orientation, and check the event calendar for upcoming training.
Safety
Follow the Metal Shop safety requirements for helmets, gloves, jackets, ventilation, and flammable materials.
- The TIG arc gives off strong ultraviolet light. Cover all exposed skin, and close the weld curtain.
- The tungsten, torch cup, and workpiece stay hot after you stop welding.
- Clean metal before welding. Do not weld galvanized, plated, or painted metal without removing the coating first.
- If the tungsten touches the weld pool or filler rod, stop and regrind or replace it. A contaminated tungsten gives an unstable arc.
Controls
Selector Switches
| Switch | Function |
|---|---|
| TIG / MMA | TIG welding or DC stick welding. |
| AC / DC | In TIG mode: AC for aluminum and magnesium, DC for steel, stainless steel, and most other metals. |
| 2T / 4T | 2T: press and hold the torch switch to weld, release to stop. 4T: press to start, release to weld, press again to start the down slope, release to stop. Use 4T for long welds without a foot pedal. |
| Pulse (Off / Low / High) | Off: standard TIG. Low and High set the pulse frequency range. |
Control Dials
These are the dials on our machine's panel, in panel order. The line drawn across the panel between the two rows shows where each setting acts during a weld.
| Dial | Range | Function |
|---|---|---|
| Start Current | 10–225A | Current when the arc strikes. Lower it for thin sheet metal. |
| Up Slope | Up to 10 s | Time to rise from start current to welding current. |
| Welding Current | 10–225A | Main amperage, shown on the AMP display. With the foot pedal connected, this sets the maximum the pedal can reach. |
| Down Slope | 0–25 s | Time to drop from welding current to end current. |
| End Current | 10–225A | Current at the end of the weld, to fill the crater. |
| AC Frequency | 40–200 Hz | In AC mode, a higher frequency gives a narrower, more focused arc. |
| AC Balance | 10–90% | In AC mode, the balance between cleaning action, which removes oxide from aluminum, and penetration. |
| Pre-Flow | Up to 3 s | Gas flow before the arc starts. |
| Base Current | Up to 95% | In pulse mode, the low current level, as a percentage of welding current. |
| Pulses Per Second | Up to 200 Hz | In pulse mode, how many times per second the current switches between peak and base. |
| Pulse Duty | From 10% | In pulse mode, how much of each pulse is at peak current. Higher gives more heat and penetration; lower is safer for thin material. |
| Post Flow | From 0 s | Gas flow after the arc stops. Protects the hot tungsten and weld while they cool. |
The O.C light next to the display comes on when the machine overheats or is overloaded. Stop and let it cool before welding again.
Setup
- Make sure the machine is off.
- Set TIG / MMA to TIG. Set AC / DC for your metal.
- Fit the tungsten. Use a collet and collet body that match the tungsten diameter, and a cup sized for the job.
- Clamp the ground to clean, bare metal close to the joint.
- Open the argon cylinder valve and set the flow on the regulator.
- Plug in the foot pedal, or set 2T / 4T to use the torch switch.
- Turn the machine on and set the welding current and post flow.
Starting Settings
These are starting points. Practice on scrap of the same material and thickness, and adjust from there.
General
- Argon flow: 15–20 CFH with a #6 or #7 cup. Use more for larger cups or drafty conditions.
- Tungsten: 2% ceriated (gray) or 2% lanthanated (blue) works for both AC and DC. Use 3/32" for most work and 1/16" for thin material under about 80A.
- Tungsten prep: For DC, grind to a point with the grind marks running lengthwise. For AC, grind a point and blunt the tip slightly.
- Pre-flow: about 0.5 seconds.
- Post flow: about 1 second per 10A of welding current, and at least 5 seconds.
- Pulse: off until you are comfortable with standard TIG.
Steel and Stainless Steel (DC)
Start at about 1A per 0.001" (thousandth of an inch) of thickness.
| Thickness | Current | Tungsten | Filler rod |
|---|---|---|---|
| 1/16" (1.6 mm) | 50–70A | 1/16" | 1/16" ER70S-2 (steel) or ER308L (stainless) |
| 1/8" (3.2 mm) | 100–130A | 3/32" | 3/32" ER70S-2 (steel) or ER308L (stainless) |
| 3/16" (4.8 mm) | 140–180A | 3/32" | 3/32" or 1/8" |
Aluminum (AC)
Aluminum needs more current than steel of the same thickness, because it conducts heat away quickly.
| Thickness | Current | Tungsten | Filler rod |
|---|---|---|---|
| 1/16" (1.6 mm) | 70–100A | 1/16" or 3/32" | 1/16" ER4043 |
| 1/8" (3.2 mm) | 120–150A | 3/32" | 3/32" ER4043 |
| 3/16" (4.8 mm) | 170–210A | 3/32" or 1/8" | 1/8" ER4043 |
- AC balance: start with about 30% cleaning (70% penetration). Add cleaning if the puddle looks dirty or peppered. Reduce it if the tungsten balls up or the bead is wide and shallow.
- AC frequency: about 100–120 Hz for general work. Higher gives a narrower, more focused arc.
- Clean aluminum with a dedicated stainless steel brush and acetone just before welding.
- Near 225A on thick aluminum, watch the duty cycle.
Shutting Down
- Let the post flow finish before you lift the torch away.
- Turn off the machine.
- Close the argon cylinder valve.
- Hang the torch and coil the leads. Let the torch cool before storing it.